G202 Early Strength Additive for Oil Well Cementing

Appearance Fineness (0.315mm sieve),%
Free flowing powder or particles ≤15.0
Water content,% Thickening time,min/40℃,19.1MPa,28min
≤8.0 ≤Original cement slurry

    description1

    Product Description

    G202 can change ion concentration to accelerate dissolving of the components while cement hydrating, to speed acting ofC3A and forming of calcium aluminous stone, therefore it can densify the structure of cement and enhance the early strengthening.

    Characteristics

    Suitable for oil/gas wells whose temperature is between 28℃~200℃ (BHCT).
    Modified from inorganic early-strength materials.
    Normal dosage: 0.8%~1.5% (BWOC), and it is not confined in a particular case.
    No chlorine ion, so it will not corrode the casing.
    Increases early strengthening of cement effectively and has no harmful influence on increasing the strengthening.
    Slight expanding effects can compensate the volume contraction of cement and can thereby improve the cementing quality of cement sheath.
    Suitable for normal and low density cement slurry.
    It can be used in shallow or middle-deep wells.
    It can be mixed without water or with water.

    Technical Specification

    The ingredients of cement slurry in the table are: JiaHua G class cement, W/C: 0.44; Water quality: distilled water; Dosage of G202:1.5% (BWOC).

    Appearance

    Free flowing powder or particles

    Fineness (0.315mm sieve),%

    ≤15.0

    Water content,%

    ≤8.0

    Initial consistency, Bc

    ≤30.0

    Thickening time,min/40℃,19.1MPa,28min

    ≤Original cement slurry

    Compression strength,MPa

    12h

    ≥5.0

    24h

    ≥14.0

    Packing, Storage

    Packaged with three-layer plastics bag with 25kg.
    To be kept away from moisture, heat and all possible damages of the packaging during transportation must be avoided. To be kept away from sour substances.
    Storage life time is two years.