Leave Your Message

G303 Fluid Loss Control Additive for Oil Well Cementing

Appearance Water content,%
Flow ability powder or particles ≤8.0
Fineness (0.315mm sieve),% Initial consistency, Bc
≤15.0 ≤30.0

    description1

    Product Description

    G303 can control fluid loss through forming right polymer film and enhancing viscosity of water phase.

    Characteristics

    Normal dosage: 0.8%~2.0% (BWOC). 
    Slight retarding effect.
    Suitable temperature: 30~120℃(BHCT),With the increase of temperature, the dosage should be increased appropriately, and supplemented with necessary retarder to adjust the thickening time.
    Low initial consistency and good rheology.
    No harmful influence on compression strength.
    Mixed without water.

    Technical Specification

    The ingredients of the cement slurry in the table are: G class cement, W/C 0.44, Dosage of G303: 1.8 % (BWOC), Water quality: distilled water.
    Items Specification

    Appearance

    Flow ability powder or particles

    Water content,%

    ≤8.0

    Fineness (0.315mm sieve),%

    ≤15.0

    Initial consistency, Bc

    ≤30.0

    Thickening linear mutation value,Be

    ≤10.0

    Transition time,min

    ≤40.0

    Fluid loss, ml/80℃,6.9MPa,30min

    ≤150.0 

    Free fluid, %/80℃

    ≤1.4

    Compression strength, MPa/102℃,21MPa,24h

    ≥14.0 

    Packing, Storage

    Be sacked with three-layer plastics bag, 25kg per bag.
    Be kept away from moisture and possible damage of the packages in transportation, and be stored in cool and dry situation. 
    Storage life time is two years.
    Leave Your Message