Leave Your Message

G309 Fluid Loss Control Additive for Oil Well Cementing

Initial consistency. Bc/80℃. 46.5MPa.45min Mutation value of thickening liner,Bc
≤30.0 ≤10.0
40Bc~100Bc, time, min Fluid loss, ml/80℃. 6.9MPa.30min
≤40.0 ≤150.0

    description1

    Product Description

    G309 can control fluid loss and expansion through forming a tight film that depends on the crystal expansion of hydratable substance.

    Characteristics

    Appearance: white powder or particles.
    Normal dosage: 0.8%~2.0%(BWOC) for normal density cement slurry, and 1.0%~3.0%(BWOC)for low density cement slurry. 
    Applicable temperature:30℃~120℃(BHCT).
    Little fluid loss, high early strength, free fluid closes to zero.
    Tiny expansion, the cement can engender effective expansion while it is in plastic phase or has been hardened. It can be used to as gas locked agent, enhance the strength of cement and cementation, densify the structure of cement.
    Good rheology of cement slurry, adjustable thickening time, thickening curve 40Bc~70Bc, short transition thickening time. 
    Mixed without water with cement equably.

    Technical Specification

    The ingredient of the cement slurry in the table is: G class cement, W/C: 0.44, Dosage of G309: 1.2% (BWOC), Water quality: distilled water.
    Items Specification

    Appearance

    white powder or particles

    Water content, %

    ≤10.0

    Fineness (0.315 mesh), %

    ≤15.0

    Initial consistency. Bc/80℃. 46.5MPa.45min

    ≤30.0

    Mutation value of thickening liner,Bc

    ≤10.0

    40Bc~100Bc, time, min

    ≤40.0

    Fluid loss, ml/80℃. 6.9MPa.30min

    ≤150.0

    Free fluid,%(80℃)

    ≤1.4

    Compression strength, MPa/102℃.21MPa.24h

    ≥14.0

    Packing, Storage

    Be sacked with three layer package, 25kg per bag.
    Be kept away from moisture, stored in cool and dry situation. 
    Storage life time is two years.
    Leave Your Message