G403 Channeling-control Toughening Additive for Oil Well Cementing

Mutation value of thickening curve,Bc Increasing flexural strength,%/75 ℃.0.1 MPa.48 h
≤10.0 ≥15.0
Increasing impact energy,%/75 ℃.0.1 MPa.48 h Compression strength, MPa/75℃,0.1 MPa,48h
≥15.0 ≥14.0

    description1

    Product Description

    G33S reduces the slurry cake permeability by the aggregation of water-soluble high polymer molecular chain. And a variety of functional groups are introduced into the polymer to enhance the anti high temperature property and salt resistance. 

    Characteristics

    Non-poisonous or non-odor;
    Normal dosage: 1.5%~2.5%(BWOC).
    No harmful on thickening time, rheological properies and free fluid control of cement slurry. Enhance compression strength obviously.
    Suitable for cement slurry with normal and low density.
    Suitable for dry mixing, can not be mixed with water.

    Technical Specification

    The ingredient of the cement slurry in the table is: JiaHua G class: cement, W/C 0.44
    Dosage of G403: 1.8%(BWOC).  Water quality: distilled water.

    Items

    Specification

    Appearance

    Free flowing powder

    Initial consistency, Bc/52℃,35M.6Pa,28min

    ≤30.0

    Mutation value of thickening curve,Bc

    ≤10.0

    Increasing flexural strength,%/75 ℃.0.1 MPa.48 h

    ≥15.0

    Increasing impact energy,%/75 ℃.0.1 MPa.48 h

    ≥15.0

    Compression strength, MPa/75℃,0.1 MPa,48h

    ≥14.0

    Packing, Storage

    Be sacked with three-layer plastics bag, 25kg per bag.
    Be kept away from acid, alkali and moisture. 
    Storage life time is two years. 